Driven by the “Dual Carbon” strategy, the new energy vehicle industry continues to grow rapidly, and the lightweight design, high safety, and high integration of power battery enclosures have become key development priorities.
Battery enclosures are primarily used to house battery cells, modules, thermal management systems, high-voltage components, and other parts.
Although steel enclosures offer high strength, their high density significantly increases the vehicle’s overall weight, which hinders efforts to extend driving range;
Meanwhile, the widespread adoption of composite material enclosures—such as those made of carbon fiber—is limited by high costs and manufacturing challenges.
Aluminum alloy, with a density of approximately one-third that of steel and excellent ductility and thermal conductivity, has thus become the ideal material choice for lightweight automotive battery enclosures.
Under highly integrated architectures such as CTB and CTC, battery housings have evolved from traditional functional components into load-bearing body structural elements.
They must simultaneously fulfill multiple functions—including load-bearing, protection, sealing, and thermal management—which presents new challenges in terms of stiffness enhancement, precision control, and multi-objective performance trade-offs.
Consequently, there is an urgent need to systematically examine aluminum alloy housing technology across three dimensions: materials, processes, and structure.
This paper focuses on aluminum alloy power battery housings, systematically reviewing their material systems, forming processes, and joining technologies.
It analyzes key performance requirements and their intrinsic relationships and outlines future development trends, with the aim of providing a reference for related research and engineering practice.
Research Progress on Aluminum Alloy Materials for Battery Cases
Aluminum alloy materials can be broadly classified into two categories: wrought aluminum alloys and cast aluminum alloys.
Manufacturers produce wrought aluminum alloys from cast ingots.
Extrusion, rolling, forging and stamping create plastic deformation in these ingots.
Cast aluminum alloys follow a different forming route. Workers pour molten aluminum into mold cavities.
The liquid metal solidifies inside the mold. This process requires no plastic deformation.
The wrought aluminum alloys suitable for power battery casings primarily include 3xxx-series Al-Mn alloys, 5xxx-series Al-Mg alloys, 6xxx-series Al-Mg-Si alloys, and the less commonly used 7xxx-series Al-Zn alloys;
Cast aluminum alloys are predominantly Al-Si-based, as shown in Table 1.
3xxx Series Deformable Aluminum Alloys
Al-Mn alloys contain manganese (Mn) as the primary alloying element, along with small amounts of iron (Fe), silicon (Si), magnesium (Mg), and other elements.
Al-Mn alloys, typified by the 3003 aluminum alloy, offer good corrosion resistance but have low strength and cannot be heat-treated for strengthening.
They are primarily used for battery liquid-cooling plates and cell casings and are generally not used in load-bearing structures.
-
5xxx Series Deformable Aluminum Alloys
Al-Mg alloys use Mg as the primary alloying element and contain small amounts of elements such as Mn and Cr.
These alloys are classified as medium-strength alloys and cannot be heat-treated for strengthening.
Representative examples include the 5052 and 5083 aluminum alloys, which are commonly used for mounting brackets, sealing plates, and other components in battery housings.
-
6xxx Series Deformable Aluminum Alloys
Al-Mg-Si alloys contain Mg and Si as their primary alloying elements, along with small amounts of Cu, Mn, Cr, and other elements.
They are classified as medium- to high-strength alloys that can be heat-treated for strengthening.
These alloys offer good machinability and are suitable for various processing methods, including extrusion, rolling, and forging; they also exhibit good corrosion resistance and excellent weldability.
Represented by grades 6061, 6063, 6082, and 6005A, these alloys are commonly used for longitudinal beams, crossbeams, and reinforcing beams in battery housing frames.
They are among the most widely used aluminum alloys and are the material of choice for welded-profile battery trays.
-
7xxx Series Deformable Aluminum Alloys
Al-Zn alloys use Zn as the primary alloying element and contain elements such as Cu and Mg.
They are high-strength alloys that can be heat-treated for strengthening and exhibit good wear resistance;
However, they have poor corrosion resistance, as well as poor weldability and a tendency to crack, and are therefore used only in localized structural reinforcements.
Represented by grades 7075 and 7050, they are primarily used in components requiring high strength, such as battery casing lug sleeves and locating pins.
-
Al-Si Series Die-Casting Aluminum Alloys
Al-Si series die-casting aluminum alloys offer excellent casting properties, low crack susceptibility and shrinkage, as well as good corrosion resistance.
These alloys are suitable for both high-pressure and low-pressure die-casting processes.
AlSi10MnMg is commonly used in high-pressure die casting and offers excellent casting fluidity and mechanical properties;
The A356 alloy, commonly used in low-pressure die casting, features excellent gas tightness, mechanical properties, and heat treatability, and is widely used.
-
Current Status of Research on New Aluminum Alloy Materials
1. Application Background and Limitations of Traditional Aluminum Alloys
Conventional wrought aluminum alloys and die-cast aluminum alloys have already been applied on a large scale in the field of power battery casings;
However, traditional alloys are gradually revealing limitations such as an insufficient balance between strength and ductility.
Power battery systems now adopt highly integrated structures. Battery enclosures must withstand bottom impact loads.
Ultra-fast charging puts forward strict thermal management requirements.
Heavy-duty trucks expose components to severe service environments.
Researchers have developed a series of advanced aluminum materials to meet these needs.
The material portfolio includes microalloyed extruded aluminum alloys.
It also covers heat-treatment-free die-cast aluminum alloys, high-thermal-conductivity functional aluminum alloys, aluminum-based composites and recycled aluminum.
These new grades have emerged steadily in recent years.
2. Microalloyed Extruded Aluminum Alloys
Lesheng et al. found that Sc microalloying of 6082 aluminum alloy (increasing Sc content from 0 to 0.7%) significantly refined the grain structure, reducing grain size from 250.8 μm to 17.8 μm and increasing tensile strength by 90.6%.
3. Heat-Treatment-Free Die-Cast Aluminum Alloys
Alcoa developed the heat-treatment-free die-casting aluminum alloy C611 by optimizing silicon content, which meets the requirements for thin-walled castings and product performance;
The heat-treatment-free JDA1 alloy developed by Shanghai Jiao Tong University increased production efficiency by 40%.
4. High-Thermal-Conductivity Functional Aluminum Alloys
High-thermal-conductivity functional aluminum alloys are primarily concentrated in the Al-Si series.
For 6063 aluminum alloy, adjusting the magnesium-to-silicon mass ratio and adding appropriate amounts of rare earth elements (such as Er, La, Ce, etc.) can enhance its thermal conductivity.
5. Aluminum-Based Composites
Aluminum-based composites can be classified into three categories based on the morphology of the reinforcing phase: particulate, fibrous, and flake.
Zhang Yubo et al. conducted research on the interfacial bonding quality of carbon fiber-reinforced aluminum-based composites.
Through process optimization, when the carbon fiber volume fraction was 2.6%, the tensile strength of the prepared composite increased by 169% compared to pure aluminum, and the carbon fiber enhancement factor reached 95.1%.
6. Recycled Aluminum
Li Ning and co-authors explained how iron-rich phases act inside recycled aluminum.
They sorted iron removal approaches into three categories. These groups cover chemical methods, physical methods and physical-field methods.
They forecast a clear development direction for this field. Future work will combine multiple techniques.
Typical combinations include boron treatment paired with electromagnetic precipitation.
Another viable scheme couples ultrasonic agitation and filtration.
Progress in Research on Aluminum Alloy Battery Housing Forming Processes
Currently, the forming processes for aluminum alloy power battery housings primarily include three categories: welded extruded profiles, one-piece die-casting, and cast-extruded composite forming.
These processes differ significantly in terms of material selection, product performance, manufacturing costs, and integration levels, and are respectively suited to different vehicle platforms and battery system architectures.
-
Extruded Aluminum Profile Joining Process
The joining of extruded profiles primarily uses 6xxx-series aluminum alloys.
Through profile extrusion and machining, combined with friction stir welding (FSW) and Cold Metal Transfer (CMT), or laser welding to join the profiles and form battery enclosures.
The aluminum alloy profile enclosures produced by this process can incorporate internal water-cooling channels, offer high design flexibility for profile cross-sections, and require low tooling costs;
They have already been implemented in mass production for passenger and commercial vehicles.
However, the large number of components and the significant total length of welds in this process make it difficult to control welding distortion and ensure airtightness.
-
Integrated Die-Casting Process
The integrated die-casting process allows structural components such as the housing side beams, front panel, bottom panel, and reinforcing beams to be formed in a single casting.
This high level of integration significantly reduces the number of parts and welding operations, resulting in high production efficiency.
It also enables localized thickening of high-stress areas, aligning with the trend toward integrated chassis design.
However, die-cast aluminum alloys have poor plasticity and limited ductility, making the parts prone to internal defects such as porosity and shrinkage, which pose a risk of brittle fracture upon impact.
Additionally, the high investment required for die-casting molds and equipment has limited the widespread adoption of integrated die-cast battery enclosures.
High-vacuum die casting adds a cavity evacuation step to the traditional die casting process, allowing the molten metal to fill the mold cavity in a near-vacuum environment.
This effectively suppresses internal porosity defects in castings and significantly improves microstructural density;
Its process characteristics meet the stringent requirements for mechanical properties and airtightness of battery housings in new energy vehicles.
-
Cast-Extrusion Hybrid Forming Process
The cast-extrusion hybrid forming process combines the technical advantages of extruded profiles and die-cast components.
The perimeter frame uses 6xxx-series extruded profiles to ensure overall toughness, while complex areas such as mounting panels and corners are formed using Al-Si-series die-cast components, which are joined via welding.
In this design, the extruded profiles bear the primary load and absorb impact energy, while the die-cast components provide localized reinforcement and connections at complex locations.
This approach requires fewer components than a fully welded extrusion assembly and involves lower tooling costs than a fully integrated die-casting solution.
In recent years, it has gradually been adopted for battery enclosures in mid- to high-end passenger vehicles.
However, this process faces challenges such as difficulties in welding dissimilar aluminum alloys and microstructural inhomogeneity at the heterogeneous joints between extruded and die-cast components.
Joints are prone to failure under alternating vibration loads; therefore, thorough Design of Experiments (DOE) validation of the welding process and joint durability is required.
-
Other Emerging Forming Technologies
Hot stamping of aluminum alloys involves heating sheet metal to achieve good plasticity, followed by stamping in a die and cooling to harden the material, thereby enhancing its properties.
This deep drawing process is suitable for aluminum alloy products with complex structures and high strength requirements, and has been tested in the manufacture of battery casings.
Semi-solid die-casting technology combines the good formability of liquid casting with the excellent mechanical properties of solid-state forging.
This technique produces substantial refinement in the material microstructure.
It enhances the mechanical properties of final parts. Engineers can simplify the whole manufacturing procedure with this approach.
The technology lowers energy consumption throughout production.
Such strengths match the sustainable and high-efficiency requirements for modern automotive manufacturing.
-
Selection of Forming Processes for Aluminum Alloy Battery Housings
Table 2 compares the forming processes for aluminum alloy battery housings.
As shown in Table 2, welding together extruded profiles is currently the most widely used and mature technical approach.
It offers advantages such as low cost, dimensional flexibility, and a short development cycle, making it suitable for Class A sedans and the vast majority of CTP-architecture vehicles;
It is currently the solution with the highest market share. Integrated die-casting is a cost-saving and efficiency-enhancing technical approach for high-end mass-produced models.
By combining multiple parts into a single component, it significantly reduces welding processes and assembly labor hours, offering advantages such as short production cycles and substantial weight reduction;
However, it requires substantial investment in equipment and tooling.
It is suitable for C-segment SUVs and high-volume models with a CTC architecture, and tooling costs must be amortized through large-scale production.
Cast-extrusion composite forming is a balanced technical solution.
This hybrid method suits large commercial vehicles like heavy-duty trucks and intricate structural joints. It leverages the large-size forming strengths of extrusion. It also takes advantage of casting to integrate complex structures. The combination delivers outstanding design flexibility.
Several emerging technologies sit at different development stages.
Hot stamping for battery enclosures demands heavy capital input and precise process control. It remains at an early industrialization stage.
Semi-solid casting merges the fast forming speed of casting with the quality level of forgings.
It may substitute selected high-pressure die-cast and extruded components.
Its narrow process window and relatively high cost block widespread application for now.
Research Progress on Aluminum Alloy Housing Joining Technologies
Aluminum alloy battery casing welds come in a variety of types, including long straight sealing welds, long continuous lap welds, and complex spatial curved welds.
Friction Stir Welding (FSW) achieves high-strength load-bearing capacity through solid-state joining;
Laser welding enables high-speed, continuous welding of thin-walled components using high energy density;
And Continuous Metal Transfer (CMT) welding achieves high-precision welding of complex frameworks with extremely low heat input.
These three methods respectively address three core operating conditions: long straight welds under heavy loads, high-speed thin-walled welding, and complex precision welding.
-
Friction Stir Welding
Friction stir welding is a solid-state joining process in which the metal does not melt during welding.
This welding process reduces pore defects in weld seams. It raises the strength of welded joints.
It limits residual deformation after joining. Manufacturers use this method broadly for battery tray liquid-cooling plates.
Han Zhenyu and his team carried out welding trials on 6063 aluminum alloy battery box lower shells.
They set high travel speeds and high rotational speeds for the tests.
They characterized the microstructure and mechanical performance of the resulting joints.
The study indicated a lack of synergy between strength and ductility improvements;
While tensile strength could consistently reach over 70% of the base material’s value, elongation tended to deteriorate within a specific process window.
Wu Feibiao et al. conducted compatibility tests on process parameters and base material joining methods using a robotic friction stir welding platform.
Through parameter optimization, they effectively improved weld quality, with the joint’s tensile strength consistently reaching at least 70% of the base material’s standard value.
Friction stir welding can produce aluminum profile joints with excellent ductility;
However, the equipment costs are high, and the flexibility of the weld path is inferior to that of laser welding.
When performing multi-pass assembly welding on large-sized frames, fixture conditions directly affect product dimensional accuracy and are not conducive to the production of complex spatial welds.
Therefore, this process is suitable for thick-walled aluminum profiles and long, straight, sealed welds, but it struggles to handle a large number of complex corner and curved weld conditions.
-
Laser Welding
Laser welding delivers high energy density, low heat input and fast welding speed.
It fits automated mass production for continuous long seams on aluminum alloy battery frames.
This process demands tight assembly tolerance for workpieces.
Dimensional deviations of incoming parts readily trigger welding defects.
Factories widely adopt single-laser or oscillating laser welding for thin-walled battery casings without load-bearing duties.
Thicker aluminum alloy sheets and extruded profiles face different limits.
Complex welding conditions and strict quality standards slow the shift from MIG welding to laser welding.
The full replacement has not taken place so far.
With the growing adoption of laser wire-fed welding or laser-arc hybrid welding, this bottleneck is expected to be resolved.
-
Cold Metal Transfer Welding
Cold Metal Transfer (CMT) welding features low heat input and is well-suited for welding thin sheets, castings, and aluminum alloy frames.
It produces minimal spatter and is the mainstream production process for aluminum alloy frames;
However, its welding speed is relatively low, resulting in insufficient production efficiency for long primary welds.
Yue Caiyue et al. compared the welding performance of CMT and MIG.
The results show that when welding 3 mm aluminum sheets, CMT produced virtually no distortion, whereas MIG caused approximately 4 mm of distortion;
When welding 8 mm aluminum sheets, CMT also exhibited less distortion.
The penetration depth of the welds for both processes was approximately 0.5 mm, with no significant difference.
The CMT process can effectively control welding distortion and is particularly suitable for welding thin sheets and aluminum alloy products with high precision requirements.
-
Other Joining Methods
In terms of mechanical joining, flow-drill screws (FDS) are widely used in the assembly of aluminum housings.
FDS enables the connection of multi-layer aluminum alloy components without pre-drilled holes, making it suitable for automated production lines;
However, the screws are relatively expensive, and there is a risk of electrochemical corrosion at the screw locations.
Structural adhesive bonding forms reliable joints between dissimilar materials.
This joining method avoids welding-induced defects such as thermal distortion and stress concentration.
The process delivers additional benefits for lightweight design. Adhesive seals the joint interface. It also absorbs in-service vibration.
Hybrid adhesive-riveted joints combine structural adhesive bonding with mechanical riveting (such as SPR/FDS).
The adhesive layer provides continuous load-bearing surfaces and uniform stress distribution, while riveting offers peel resistance and impact resistance.
This complementary combination increases the joint’s shear strength to more than twice that of pure riveting and improves energy absorption by 45%.
Additionally, the adhesive layer fills gaps to provide sealing and corrosion protection.
This method has been widely adopted for joining cold-formed panels to frames in battery pack housings and is a key process for lightweighting automotive battery housings.
As shown in Table 3, FSW is irreplaceable for thick-walled, long, straight, high-load welds due to its solid-state joining advantages;
Laser welding offers the best cost-effectiveness for thin-walled, high-speed automated production lines;
And CMT excels at controlling deformation in high-precision, complex thin-sheet frames.
Engineering selection should be based on a comprehensive evaluation of wall thickness, weld path, production cycle time, and precision requirements.
In the mass production of large battery housings, a multi-component composite joining solution—typically “FSW (long, straight primary seam) + laser/CMT (secondary seams and complex contours) + FDS + structural adhesive”—is commonly adopted to balance strength, efficiency, and sealing performance.
Key Performance Characteristics of Aluminum Alloy Battery Enclosures
New energy vehicle battery systems keep moving toward integrated designs.
These systems must serve more complex and severe working scenarios.
Engineers no longer treat lightweighting as the only target for aluminum alloy battery enclosures.
They balance multiple critical performance indicators in the updated design framework.
These indicators include bottom impact resistance and vibration-fatigue endurance.
They also cover airtight integrity, multi-condition corrosion resistance, and thermo-mechanical coupling behavior.
Specifically, impact resistance is designed to protect the battery from compression during collisions and reduce the risk of fire;
Vibration fatigue durability ensures structural integrity during long-term operation;
Airtight reliability prevents the ingress of moisture and dust throughout the entire lifecycle;
Corrosion protection safeguards the housing against salt spray and electrolyte corrosion;
And thermo-mechanical coupling performance ensures that thermal stresses do not cause failure during high-power fast charging.
Together, these performance characteristics cover the full range of failure modes in the battery casing’s lifecycle, from “instantaneous extreme loads” to “long-term service degradation.”
-
Impact Resistance
Impact resistance primarily tests the battery enclosure’s ability to resist deformation caused by bottom impacts, bottom-support impacts, and stone impacts;
It is a core indicator of a battery system’s crash safety.
One-piece die-cast enclosures form complex structures in a single step.
High-silicon aluminum alloys used for these parts show limited ductility.
Casting porosity defects easily appear inside the material. These flaws raise the risk of brittle fracture under bottom impact loads.
Heat-treatment-free die-cast aluminum alloys and high-vacuum die-casting processes can improve their impact resistance to a certain extent.
Extruded and welded battery enclosures use 6xxx-series aluminum alloy profiles, which offer good overall resistance to vibration, compression, and impact;
However, their weak points are often located in the heat-affected zones of the welds.
Processes such as oscillating laser welding and friction stir welding can effectively improve the toughness of the joints, thereby enhancing the overall impact resistance of the enclosure.
-
Vibration Fatigue Durability
Commercial vehicle battery housings are subjected to multidirectional random vibration loads during service, with welded joints, threaded connections, and interfaces between dissimilar materials being high-risk areas for fatigue failure.
To address the frequent jolting conditions experienced by heavy-duty trucks, measures such as flexible connections or the application of threadlocker can help reduce the risk of fastener loosening and frame fracture.
In terms of structural optimization, adding reinforcing ribs through topological optimization can effectively increase local modal frequencies, thereby preventing fatigue failure caused by resonance.
-
Air Tightness and Seal Reliability
Seal reliability is a fundamental performance requirement for power battery casings.
It ensures the safe operation of the battery system by isolating it from external moisture and dust and preventing electrolyte leakage.
Battery casings generally must pass an IPX8 submersion test (1 m water depth, 48 hours);
Common testing methods include the pressure differential method, flow rate method, and helium leak detection.
Leaks primarily occur at weld seams and assembly interfaces; welding defects, out-of-tolerance flatness, and sealant aging can all lead to failure to meet airtightness standards.
During the battery casing development phase, structural design, material selection, and process optimization should be coordinated to reduce the risk of leaks.
Assembly tolerances should be controlled prior to welding, and 100% airtightness testing should be performed using a leak detector after welding to ensure the sealing performance of the battery casing throughout its entire lifecycle.
-
Corrosion Protection Performance
Corrosion protection encompasses two categories: atmospheric salt spray corrosion and electrolyte corrosion.
During service, aluminum alloy housings are continuously exposed to road de-icing salts, muddy water, and humid air.
Aluminum-steel threaded joints appear widely at grounding bolts and mounting positions.
A potential gap of roughly 0.8–1.0 V develops between these two metals.
This difference triggers galvanic corrosion at the contact interface.
An electrolyte film speeds up the dissolution of the aluminum anode.
Electrolyte leakage caused by cell thermal runaway or mechanical damage can induce pitting corrosion on the casing;
In severe cases, this can lead to perforation and failure of a 2–3 mm-thick casing within a matter of weeks.
Aluminum alloy battery casings are typically required to pass a neutral salt spray test for ≥ 720 h (with no substrate corrosion) and a copper-accelerated acetic acid salt spray test (CASS) for ≥ 144 h.
Protective measures such as electrical insulation, protective coatings, or buffering agents must be applied to the casing;
During product development, structures prone to the accumulation of corrosive media—such as narrow gaps and dead corners where water can pool—should be avoided, and drainage holes should be appropriately positioned.
-
Thermal-Mechanical Coupling Performance
1. Thermo-Mechanical Coupling Risks Under High-Power Fast Charging
High-power fast charging sees broader adoption across the industry.
Batteries generate heat much faster during charge and discharge cycles.
Thermo-mechanical coupling challenges grow more serious for aluminum alloy battery enclosures.
Battery enclosures serve a dual function: providing structural support and facilitating heat conduction and dissipation.
During actual vehicle operation, the heat generated by fast charging combined with seasonal temperature fluctuations results in frequent high-to-low temperature cycles.
This causes continuous alternating thermal stresses in the enclosure, welds, and sealing interfaces, which act on vulnerable areas such as welded joints and assembly sealing surfaces.
This accelerates fatigue damage at weld points, causes stress fluctuations at sealing interfaces, and increases the risk of seal failure.
2. Multi-Performance Balancing Requirements for Enclosure Design
Engineers face this key requirement at the enclosure design stage.
They must reconcile thermal management and cooling demands. They also need to maintain structural strength and fatigue resistance.
Careful balancing delivers coordinated performance across multiple dimensions.
In summary, these five key performance characteristics are not independent of one another;
Rather, they are interconnected through a multi-objective coupling and mutual constraints involving “strength—toughness—durability—corrosion resistance—thermal management.”
3. Existing Technical Routes for Battery Enclosure Development
Current housing development leverages topological optimization to achieve a balance between weight reduction and performance while meeting strength and stiffness constraints;
It uses gradient materials and composite structures (such as honeycomb sandwich panels and foam aluminum fillers) to locally enhance impact and fatigue resistance in critical areas;
Engineers use multi-modal composite joining schemes.
A typical combination includes FSW main seams, laser or CMT auxiliary seams, FDS fasteners and structural adhesive.
This combination balances structural strength, production speed and sealing capacity.
Adhesive layers fill interfacial gaps between joined components.
These adhesive layers support sealing and corrosion resistance. They also redistribute local stress on the joint.
In the future, battery casing development will shift from optimizing individual metrics toward an integrated, collaborative design approach encompassing “materials—structure—process.”
Outlook
Material innovation, manufacturing upgrades and system integration jointly shape the future of aluminum alloy battery enclosures.
These three pillars form the core of its coordinated evolution.
New material breakthroughs expand achievable performance limits.
Updated manufacturing processes turn these performance targets into reality.
System integration reshapes the functional positioning of the enclosure itself.
Each element supports and accelerates the other two.
Their mutual advancement pushes enclosure technology toward better performance, reduced cost and improved sustainability.
-
Materials Perspective
Currently, battery casings in mass production are still primarily made from traditional 6xxx-series extruded aluminum alloys and die-cast aluminum alloys such as AlSi10MnMg and A356.
Novel aluminum materials cover microalloyed extruded profiles, heat-treatment-free die-casting alloys and high-thermal-conductivity functional aluminum alloys.
These materials will gradually break cost and process limits. They will see wider use in engineering practice.
Recycled aluminum will account for a larger share of raw materials.
This shift supports industrial low-carbon targets. Manufacturers still face two urgent bottlenecks.
They must stabilize recycled aluminum quality. They also need a complete supporting system of material standards.
-
At the Manufacturing Process Level
Integrated die casting will continue to evolve toward larger dimensions, higher toughness, and heat-treatment-free production;
Extrusion-welding and cast-extrusion composite forming processes will further enhance mass production quality stability through upgrades to welding equipment and optimizations in deformation control technology.
Emerging processes such as HFQ hot stamping and semi-solid die casting are unlikely to fully replace mainstream forming processes in the short term;
They are primarily suited for the manufacture of specialized or small-batch housings.
Joining technologies are shifting from single-welding methods toward hybrid welding-mechanical connections to reduce welding risks and enhance joint reliability.
-
Structural and Functional Integration and Standardization
CTB and CTC architectures gain wider deployment. Battery enclosures will carry structural loads for the whole vehicle.
Designers merge water-cooling channels and fire-resistant structures into these enclosures.
This integration delivers one solution for structural support, thermal control and thermal runaway containment.
Heavy-duty trucks and construction machinery create harsh service environments.
Engineers must coordinate material selection, structural layout and joint design.
This coordinated work guarantees reliable performance over the full service life.
The industry also pushes platform-based battery pack development and standardization.
Unified material datasets, joining specifications and design rules form the foundation.
These resources realize universal interfaces and consistent manufacturing workflows.
Developers shorten lead times and cut overall costs. They also improve component reuse across different product platforms.
R&D teams will adopt digital twins and multi-physics simulation tools.
These tools narrow the gap between physical tests and numerical predictions. They speed up the whole research and development cycle.
-
Green Design and Repairability/Recyclability
Green design and recyclability will become key trends in the development of battery enclosures.
Although integrated die-casting offers a compact structure, it has poor repairability; in the future, a balance will need to be struck between integration and disassembly.
Regulatory rules for battery recycling set new constraints for the industry.
Material carbon footprint tracking emerges as a core requirement.
Design schemes will prioritize easy disassembly. Recycled aluminum will see expanded application.
These three directions guide future technical development.
Conclusion
This paper provides a systematic review of research progress on aluminum alloy battery casings in terms of materials, forming processes, joining technologies, and key performance characteristics.
The main conclusions are as follows:
-
Material Systems
6xxx-series aluminum alloys are the material of choice for welded profiles due to their balanced overall properties;
Al-Si-based alloys are well-suited for die-casting processes and form the foundation for integrated designs;
7xxx-series alloys are primarily used for localized reinforcement.
Microalloying, heat-treatment-free alloys, high-thermal-conductivity alloys and recycled aluminum dominate new material research.
Recycled aluminum still requires technical breakthroughs to maintain stable quality.
-
Forming Processes
Extrusion-welding, integrated die-casting, and cast-extrusion composite forming will coexist for the foreseeable future.
Extrusion-welding stands out for its low cost and strong flexibility.
Integrated die-casting cuts costs and boosts efficiency for highly integrated CTB and CTC designs.
High mold and equipment expenses restrict its broader rollout.
Cast-extrusion composite forming fits heavy-duty trucks and enclosures with complex structures.
Hot stamping and semi-solid die-casting remain at the early industrialization stage.
-
Joining Technologies
FSW is suitable for thick-walled, long, straight, high-load-bearing welds;
Laser welding offers the best cost-effectiveness in thin-walled, high-speed production lines; CMT excels in deformation control;
And FDS combined with structural adhesive is a key process for joining cold plates in battery enclosures.
Currently, most enclosures employ multi-modal composite joining solutions;
-
Key Performance Aspects
Enclosure design now targets simultaneous optimization across multiple metrics.
These metrics cover strength, toughness, durability, corrosion resistance and thermal management.
Designers use several strategies to reach balanced performance. Topology optimization helps refine structural layouts.
Gradient materials and composite structures tailor local properties.
Multi-modal composite joining delivers reliable multi-function joints.
In the future, battery enclosure design will evolve from single-performance optimization toward integrated, collaborative design encompassing “materials, structure, and process.”